Epoxy repair kit NEW

Home » Prodotti » Resine » Epoxy repair kit NEW
Sea Line farby jachtowe
Epoxy repair kit NEW

DESCRIZIONE DEL PRODOTTO :

Per ottenere una laminazione di massima qualità e adeguata durezza usare una miscelazione 2:1 in peso per la fibra di vetro mate, se si utilizza il tessuto di vetro miscelare in rapporto 1:1 in peso.


INFORMACIONI DI BASE:

TIPOlaminazione, legno, alluminio, acciaio
Postosotto e sopra la linea di gallegg
Miscelazione a volume10 :50
Miscelazione a peso100 : 44
Durata della miscela a 20°C45 minutti
Tempo di indurimento a 20°C7 ore

CONFEZIONE :

250 g /  CODICE : 3636

IN CONFEZIONI DA :

APPLICAZIONE:

Manualmente:

INFORMAZIONI TECNICHE :


Condividi:

Avete domande?
Ti risponderemo il prima possibile
 
Vedi anche
Altri prodotti in questa categoria

Le nostre FAQ
Risposte alle domande più frequenti

Why did the polyurethane topcoat become dull?

Possible causes

  • Too short time for evaporation of the thinner,

How to prevent

  • Maintain the right conditions for complete evaporation of the thinner,

How to remove

  • Mat the surface, degrease and apply the paint according to the rule (right conditions and thinning proportions)
  • Polish surface if needed.

Do you have to paint the scratched side of the boat?

If the scratches are not deep, then we can renew the scratched side by polishing with Sea-Line polishing pastes. Above the waterline, when the scratches are not deep, the surface can be repaired with a DRY FAST gel coat filler. Deep scratches should be filled with epoxy filler (selected depending on the requirements of the scratched surface), painted with a primer and then painted with topcoat.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.