Linguaggio:

HARD ANTIFOULING

Home » Prodotti » Antivegetativa » HARD ANTIFOULING
Sea-Line
HARD ANTIFOULING

HARD ANTIFOULING paint:


Use biocides safely. Always read the label and product information before use.

Type GRP laminates, wood, Steel
Place Below waterline
Function Antifouling paint discourages the growth
of barnacles, weed, and other water life on the
submersed hull of the boat.
Application brush, roll, spray gun
Thinning *No recommended
Theoretical coverage For 1l± 10 m2 for
90 μmWFT/ 50 μm DFT
Coats number 1 – 3
 Maximum recommended layer thickness100 μm DFT
Time between layers Min 6 h
Dry to launch: Min 12 h
Pack0,750 l2,5 l
Color **codecode
Black

Red

Dark Blue

8282

8286

8284

8287

8289

8288

* THINNING NOTICE:

In the case of high temperatures and the need to thin the antifouling paint, a maximum dilution of 0-5% (by volume) is recommended.
Dilution and the application method directly affect the thickness of the antifouling paint layer.

Special attention should be paid to obtaining a specific coating thickness (100 μm DTF), which ensures the effective operation of the antifouling paint.

** COLOR NOTICE:

Exposure of a freshly applied antifouling paint to moist air can lead to color change. The discoloration is only superficial and does not affect the effectiveness of the antifouling paint. Due to the content of copper oxide, a small color difference between the parts of the antifouling paint is acceptable.


Condividi:

Avete domande?
Ti risponderemo il prima possibile

Prodotti correlati

da HARD ANTIFOULING


Vedi anche
Altri prodotti in questa categoria

Le nostre FAQ
Risposte alle domande più frequenti

Why did the polyurethane topcoat become dull?

Possible causes

  • Too short time for evaporation of the thinner,

How to prevent

  • Maintain the right conditions for complete evaporation of the thinner,

How to remove

  • Mat the surface, degrease and apply the paint according to the rule (right conditions and thinning proportions)
  • Polish surface if needed.

Do you have to paint the scratched side of the boat?

If the scratches are not deep, then we can renew the scratched side by polishing with Sea-Line polishing pastes. Above the waterline, when the scratches are not deep, the surface can be repaired with a DRY FAST gel coat filler. Deep scratches should be filled with epoxy filler (selected depending on the requirements of the scratched surface), painted with a primer and then painted with topcoat.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,
La nostra offerta
Familiarizzate con la nostra offerta di materiali e vernici per la costruzione di barche
Exit
Przewiń na górę