MULTIFUNCTIONAL 2K SPRAY EPOXY PRIMER

Home » Prodotti » Primers » MULTIFUNCTIONAL 2K SPRAY EPOXY PRIMER
Zabezpieczenie łodzi
MULTIFUNCTIONAL 2K SPRAY EPOXY PRIMER

EPOXY PRIMER MULTIFUNCTIONAL 2K SPRAY

PRODUCT DISCRIPTION:



BASIC INFORMATION:

SurfacesGRP, laminates, steel, aluminum
AreaAbove and below waterline
FunctionGrounding
Intercoating
Filling
Antiosmotic
Anticorosive
Applicationspray can
Theoretical coverage for 400 ml 1-2 м2
Number of coats2 – 4
Pot life 20°C48 h
Time between layers without sanding5~10 minutes
Color (matt)white
Pack400 ml
Code 38758

APPLICATION INSTRUCTION:

potrzasnij

Before triggering, shake can thoroughly for 2 minutes after agitation balls are heard.

spray 2K - korek

Remove the red pushbutton from the cap.
Turn the can by 180° and fit the pushbutton onto the pin in the base of the can.

spray 2K - wcisnij korek

Turn the can upside down and place on a firm surface.
Press the red pushbutton all the way in with the palm of your hand.

potrzasnijAfter triggering, shake can again thoroughly for 2 minutes after agitation balls are heard.

spray 2K - ustaw dysze

Set the adjustable spray nozzle to the size of the damage and damage pattern.

spray 2K - aplikacja

Spray distance: 10 ~ 20cm.

spray 2K - ilosc warstw

Standard application: approx. 2÷4 spray coats, recommended dry film layer: 80 ~200 μm
NOTICE: For antiosmosis and anticorrosion protection recommended DTF is 240 μm.

spray 2K - czas

Allow a flash-off time of approx. 5-10 minutes between spray coats.

spray 2K - oczysc

After painting, turn the can upside down and spray the valve until empty.

spray 2K - utylizacja

The completely empty spray cans can be disposed of in the recycling waste container.
Cans with hardened material must be disposed of as special waste.

TECHNICAL INFORMATION:


Condividi:

Avete domande?
Ti risponderemo il prima possibile

Prodotti correlati

da MULTIFUNCTIONAL 2K SPRAY EPOXY PRIMER


Vedi anche
Altri prodotti in questa categoria

Le nostre FAQ
Risposte alle domande più frequenti

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.

Why did the polyurethane topcoat become dull?

Possible causes

  • Too short time for evaporation of the thinner,

How to prevent

  • Maintain the right conditions for complete evaporation of the thinner,

How to remove

  • Mat the surface, degrease and apply the paint according to the rule (right conditions and thinning proportions)
  • Polish surface if needed.

Can I use universal thinner?

We do not recommend using universal thinners. The use of a thinner with an unknown composition may result in loss of adhesion, lack of proper flow of paint and varnish defects.