TypeLaminates GRP, wood, steel
PlaceAbove waterline
FunctionHigh gloss
Applicationbrush, roll, spray gun
ThinningThinner for 1 – component primer, varnisch, enamel
Theoretical coverage for 1l15-16 m2 for 60 μm WFT/ 40 μm DFT
Number of coats1 ÷ 2
Dry to the touch 20°C:3 h
Dry to rain 20°C:6 h
Fully woterprof10 h
Elapsed time before applying next coat:min. 16 h
Pack0,750l125 ml
Color:code:code:
Phure white 81548166
Crem8152 –
Flame red8158 –
Gentiale blue8161 –
Jet black8163 –

During paint job is recommend to use products from one batch


Condividi:

Avete domande?
Ti risponderemo il prima possibile
 
Vedi anche
Altri prodotti in questa categoria

Le nostre FAQ
Risposte alle domande più frequenti

Is it necessary to always sand the surface between application of two different products?

We recommend to always sand the surface between applying two different products to ensure uniform surface roughness and adhesion of subsequent layers. The sanded surface should also be cleaned and degreased.

Contamination in topcoat paint?

Possible causes

  • Inaccurate surface cleaning before paint application,
  • Incorrect painting tools preparation (brush and roll),
  • Performing work in a place exposed to constant contact with dust.

How to prevent

  • Careful surface preparation (grinding, clearing, degreasing),
  • Careful painting tools preparation before use,
  • Maintain clean work environment

How to remove

  • Grind, clean and paint again.

Why despite the use of antifouing paint the bottom of the boat is overgrown?

Possible causes

  • Too thin layer of antifouling paint,
  • Choosing the wrong antifouling to type of a boat or yacht
  • Thinning of antifouling paint,
  • Incorrect surface preparation before antifouling application.

How to prevent

  • Apply the right layer thickness of paint indicated by manufacturer,
  • Choose antifouling dedicated to type of boat or yacht and suitable for the type of water,
  • Do not thin antifouling because of the risk of reducing effectiveness,
  • Careful surface preparations (grinding, clearing, degreasing),

How to remove

  • Wet grinding, apply new layers of antifouling paint.
  • Use C1 shell and fouling remover.