We starting new year with new product – polishing compound S08 INDUSTRIAL FORCE CUT.

Why S08 INDUSTRIAL FORCE CUT ?
This polishing compound have one the highest cut level, it allows to remove defects after using sand paper P600. It can be used on hardest surfaces, finished products made of laminate and for molds. Polishing compound will be especially used for light-colored surface.

For whom S08 INDUSTRIAL FORCE CUT ?
S08 INDUSTRIAL FORCE CUT was designed for manufacture which want to in fast way prepare products for next stage of productions.

Advantages S08 INDUTRIAL FORCE CUT :

All details about product are HERE (click)


Condividi:

Vedi anche
Altre discussioni in questa categoria

Le nostre FAQ
Risposte alle domande più frequenti

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.

Can I paint the bottom of the boat with polyurethane paint?

Yes, you can paint the bottom of the boat with polyurethane paint due to its high mechanical strength. We recommend this solution when the boat is not launched for a long time and is not exposed to fouling.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,