Language:

Epoxy resin NEW

Home » Products » Resins and repair kit » Epoxy resin NEW
Farby szkutnicze
Epoxy resin NEW


TypeLaminates, wood, steel, aluminum
PlaceAbove and below waterline
FunctionLaminating, repairs, reinforcement, gluing
ApplicationBrush, roll
ThinningNot recommended
 Theoretical coverage for 1kg

(for 1 layer laminate)

performance for layer of laminate based on glass fibre mats
300 g/m²

450 g/m²

~1,7 m²

~1,1 m²

performance for layer of laminate based on glass fabric (roving)
200 g/m²

400 g/m²

~5 m²

~2,5 m²

Coats numberDepend on needs
Pot life 23°C45 min
Hardening time7 h
ColorTransparente
Packcode
250 g –

500 g –

0,9 kg –

5,0 kg –

3636

8483

8508

8506 (comp. A) / 8507 (comp. B)

The resin is available in 3 sets:

Set of 250 g
-includes an epoxy resin with hardener, fabric glass (0,25 m 2), disposable gloves, a brush and a cup with a scale for easy dosing of ingredients and instructions for repair.
Set of 0,9 kg
-includes an epoxy resin with hardener

Set of 0,5 kg and 5,0 kg
-includes an epoxy resin with hardener


Share:

Do you have any questions?
We will respond as soon as possible
 
See also
Other products in this category

Our FAQ
Answers to frequently asked questions

Can I add more hardener to speed up the reaction?

Do not add more hardener, because after the base has cured, the remaining hardener will react with subsequent layers, which will be applied to the surface and cause defects. For the product to work properly, please follow the proportions given by the manufacturer.

Why despite the use of antifouing paint the bottom of the boat is overgrown?

Possible causes

  • Too thin layer of antifouling paint,
  • Choosing the wrong antifouling to type of a boat or yacht
  • Thinning of antifouling paint,
  • Incorrect surface preparation before antifouling application.

How to prevent

  • Apply the right layer thickness of paint indicated by manufacturer,
  • Choose antifouling dedicated to type of boat or yacht and suitable for the type of water,
  • Do not thin antifouling because of the risk of reducing effectiveness,
  • Careful surface preparations (grinding, clearing, degreasing),

How to remove

  • Wet grinding, apply new layers of antifouling paint.
  • Use C1 shell and fouling remover.

Contamination in topcoat paint?

Possible causes

  • Inaccurate surface cleaning before paint application,
  • Incorrect painting tools preparation (brush and roll),
  • Performing work in a place exposed to constant contact with dust.

How to prevent

  • Careful surface preparation (grinding, clearing, degreasing),
  • Careful painting tools preparation before use,
  • Maintain clean work environment

How to remove

  • Grind, clean and paint again.
Our offer
Familiarize yourself with our offer of boatbuilding materials and paints
Exit
Przewiń na górę