Lengua:

YACHT ENAMEL 1K

Página web » Productos » Capas de acabado » YACHT ENAMEL 1K
Zabezpieczenie łodzi
YACHT ENAMEL 1K


TypeLaminates GRP, wood, steel
PlaceAbove waterline
FunctionHigh gloss
Applicationbrush, roll, spray gun
ThinningThinner for 1 – component primer, varnisch, enamel
Theoretical coverage for 1l15-16 m2 for 60 μm WFT/ 40 μm DFT
Number of coats1 ÷ 2
Dry to the touch 20°C:3 h
Dry to rain 20°C:6 h
Fully woterprof10 h
Elapsed time before applying next coat:min. 16 h
Pack0,750l125 ml
Color:code:code:
Phure white 81548166
Crem8152 –
Flame red8158 –
Gentiale blue8161 –
Jet black8163 –

During paint job is recommend to use products from one batch


Compartir:

¿Tienes alguna pregunta?
Le responderemos lo antes posible
 
Ver también
Otros productos de esta categoría

Nuestras FAQ
Respuestas a las preguntas más frecuentes

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.

Why did the polyurethane topcoat become dull?

Possible causes

  • Too short time for evaporation of the thinner,

How to prevent

  • Maintain the right conditions for complete evaporation of the thinner,

How to remove

  • Mat the surface, degrease and apply the paint according to the rule (right conditions and thinning proportions)
  • Polish surface if needed.

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.