Lengua:

Sistema de pulido

Página web » Descargas » Sistema de pulido
Kosmetyki do naprawy łodzi oraz jachtów
NOMBRE DEL ARCHIVODESCARGAS
TDSSDS
S0 – FAST CUT & MEDIUM GLOSSdescargasdescargas
S05 – ONE STEP, HEAVY CUT & GLOSS (for gelcoat)downloaddescargas
S07 – HEAVY CUT (for gelcoat)downloaddescargas
S08 – INDUSTRIAL FORCE CUTdownloaddescargas
S1 – SOFT CUT & GLOSS (Liquid)descargasdescargas
S1 PREMIUM – ONE STEP, CUT & HIGH GLOSSdownloaddescargas
S2 – EXTRA SHINE HOLOGRAM REMOVER (acabado de pulido)descargasdescargas
S3 – FINISH CLEANER (shine control)downloaddescargas
S4 – PROTECT WAXdownloaddescargas
S5 – QUICK WAXdownloaddescargas

Nuestras FAQ
Respuestas a las preguntas más frecuentes

Can I purchase products directly from you?

We do not sell retail. Our products can be found in many stores in Poland and abroad. Our distributors run stationary and online stores. The full list of distributors and contacts can be found on our website at the following link click here.

Why despite the use of antifouing paint the bottom of the boat is overgrown?

Possible causes

  • Too thin layer of antifouling paint,
  • Choosing the wrong antifouling to type of a boat or yacht
  • Thinning of antifouling paint,
  • Incorrect surface preparation before antifouling application.

How to prevent

  • Apply the right layer thickness of paint indicated by manufacturer,
  • Choose antifouling dedicated to type of boat or yacht and suitable for the type of water,
  • Do not thin antifouling because of the risk of reducing effectiveness,
  • Careful surface preparations (grinding, clearing, degreasing),

How to remove

  • Wet grinding, apply new layers of antifouling paint.
  • Use C1 shell and fouling remover.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,
Nuestra oferta
Consulte nuestra oferta de materiales y pinturas para la construcción de embarcaciones
Exit
Przewiń na górę