Considering new regulations in several European countries we would like to adjust our products to current expectations.

We are ready to offer you low styrene and styrene free products:

– filler universal styrene free

– filler with fiberglass styrene free

– filler lightweight styrene free

– gelcoat filler styrene free

– filler universal styrene redced

– filler with fiberglass styrene reduced

Basic technical data here.

Please contact us in case of any questions

tel. (+48) 94 35 316 20;
SKYPE: sea-line.eu

EMAIL: info@sea-line.eu


Partager:

Voir aussi
Autres threads de cette catégorie

Notre FAQ
Réponses aux questions fréquemment posées

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.
Notre offre
Familiarisez-vous avec notre offre de matériaux et de peintures pour la construction de bateaux
Exit
Przewiń na górę