Language:

YACHT VARNISH 1K

Home » Products » Topcoats » YACHT VARNISH 1K
Szpachlówki i podkłady szkutnicze
YACHT VARNISH 1K


Typewood
PlaceAbove waterline, interior
FunctionHigh gloss
Applicationbrush, roll, spray gun
ThinningThinner for 1 – component primer, varnisch, enamel
Theoretical coverage for 1l12-13 m2 for 80 μm WFT/ 40 μm DFT
Number of coats1 ÷ 3 – renewal old varnish

1 ÷ 5 – new wood, creating new coat

Dry to the touch 20°C:3 h
Dry to rain 20°C:16 h
Fully woterprof24 h
Elapsed time before applying next coat:min. 16 h
Color:transparent
Pack :0,750 l
Code:300008170

Share:

Do you have any questions?
We will respond as soon as possible
 
See also
Other products in this category

Our FAQ
Answers to frequently asked questions

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.

Do you have to paint the scratched side of the boat?

If the scratches are not deep, then we can renew the scratched side by polishing with Sea-Line polishing pastes. Above the waterline, when the scratches are not deep, the surface can be repaired with a DRY FAST gel coat filler. Deep scratches should be filled with epoxy filler (selected depending on the requirements of the scratched surface), painted with a primer and then painted with topcoat.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.
Our offer
Familiarize yourself with our offer of boatbuilding materials and paints
Exit
Przewiń na górę