Epoxy repair kit

This is the Sea-Line epoxy repair kit, designed for repairing minor damages to boat parts.

The epoxy repair kit contains essential products that enable you to carry out the repair.

WeightCode
250 g300003636
Epoxy repair kit

Color

  • Clear

Application method

Manually:

  • brush
  • roller

Product description "Epoxy repair kit"

Sea-Line® structural epoxy is a comprehensive application:

  • It works in both the construction and repair of damaged parts of the boat.
  • This resin is recommended for laminating, sealing, enhancing the surface, bonding and linking the various elements of the structure.
  • In conjunction with the glass mat, it is used for manual repairs of substantial damage.
  • The coating has very good adhesion to any type of substrate and very high resistance and hardness.
  • Component A and B is colorless.

To obtain a full-fledged and adequately strong laminate, use a 2:1 weight ratio of resin to fibre glass mat for epoxy or a 1:1 weight ratio of resin to glass fabric.

To finish laminated surfaces we recommend using Sea-Line® epoxy fillers, Sea-Line® epoxy primers and Sea-Line® topcoats.

The resin is available in three sets:

  • epoxy resin with hardener
  • fabric glass (0,25 m 2)
  • disposable gloves
  • a brush and a cup with a scale for easy dosing of ingredients
  • instructions for repair

Basic information

TypeLaminates, wood, steel, aluminium
PlaceAbove and below waterline
FunctionLaminating, repairs, reinforcement, gluing
AplplicationBrush, roll
Coats numberDepend on needs
Pot life 23°C45 min
Hardening time7 h

You have questions about the product - Epoxy repair kit

    Also check

    Our FAQ answers to frequently asked questions

    Can I paint a boat, previously painted with 1 component paint, with polyurethane?

    It is not recommended to apply 2K paints over 1K paints. 1K and 2K inks differ in their composition and properties, including hardness, chemical resistance and durability. 1K paints are one-component and dry by evaporating the solvent, while 2K paints are two-component and need to be cured by adding a hardener. Applying 2K paint over 1K paint can cause unpredictable chemical reactions and lead to undesirable effects such as dulling, chipping or flaking of the paint. Therefore, always use paints according to the manufacturer’s instructions and do not mix different types of paints. farby zgodnie z instrukcjami producenta i nie mieszać różnych rodzajów farb.

    Can I use selfpolishing Sea-Line and HARD Sea-Line antifoulings on aluminium boat?

    Sea-Line HARD and Sea-Line self-polishing antifouling are not intended for aluminum surfaces. They include copper oxide, which in contact with aluminum causes galvanic corrosion. Especially on aluminum, we offer ALU-PLUS self-polishing anti-fouling paint, which, in addition to excellent adhesion to aluminum, is also 30% more effective than traditional anti-fouling paints.

    Why the epoxy filler does not harden?

    Possible causes

    • Incorrect proportion of base and herdener,
    • Too low temperature of ambient and surface (less than 10ﹾC),
    • Mixing two components from two different manufacturers,

    How to prevent

    • Apply the correct proportions of components
    • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
    • Use base and hardener from the same manufacturer

    How to remove

    • The uncured mass requires complete removal from the surface.