Type | GRP laminates, wood, Steel | |
Place | Below waterline | |
Function | Antifouling paint discourages the growth of barnacles, weed, and other water life on the submersed hull of the boat. | |
Application | brush, roll, spray gun | |
Thinning * | No recommended | |
Theoretical coverage For 1l | ± 10 m2 for 90 μmWFT/ 50 μm DFT | |
Coats number | 1 – 3 | |
Maximum recommended layer thickness | 100 μm DFT | |
Time between layers | Min 6 h | |
Dry to launch: | Min 12 h | |
Pack | 0,750 l | 2,5 l |
Color ** | code | code |
Black Red Dark Blue | 8282 8286 8284 | 8287 8289 8288 |
In the case of high temperatures and the need to thin the antifouling paint, a maximum dilution of 0-5% (by volume) is recommended.
Dilution and the application method directly affect the thickness of the antifouling paint layer.
Special attention should be paid to obtaining a specific coating thickness (100 μm DTF), which ensures the effective operation of the antifouling paint.
Exposure of a freshly applied antifouling paint to moist air can lead to color change. The discoloration is only superficial and does not affect the effectiveness of the antifouling paint. Due to the content of copper oxide, a small color difference between the parts of the antifouling paint is acceptable.
It is very important to use paint thinners, which provide the appropriate parameters of paint – flow, pot life, time […]
Self – polishing Antifouling ALU PLUS protect areas below the water line. It can be applied on aluminium (light alloy), […]
Suitable for salty and regular water. Suitable for sailing and motor boats traveling with a maximum speed 40 knots. For […]
Silver Speed HARD Antifouling is a hard antifouling paint, effectively preventing fouling organism: aquatic plants and animals or slime. Ideal […]
If the scratches are not deep, then we can renew the scratched side by polishing with Sea-Line polishing pastes. Above the waterline, when the scratches are not deep, the surface can be repaired with a DRY FAST gel coat filler. Deep scratches should be filled with epoxy filler (selected depending on the requirements of the scratched surface), painted with a primer and then painted with topcoat.
Yes, you can mix Sea-Line polyurethane paints. The only difference are the pigments of polyurethane paints that determine the color of the paint. But remember to keep the right proportions of base, hardener and thinner.
Il patch e compensare le irregolarità derivanti da danni durante la produzione
Barca protezione superficiale contro l’influenza di azioni distruttive di osmosi e la corrosione in ambienti difficili
Protezione contro l’acqua e contro gli effetti negativi delle radiazioni UV
Proteggere la parte inferiore della barca prima-tedesco ricoperta di alghe e conchiglie. La prevenzione dell’azione di acqua.
Rimozione efficace di ritenzione graffi, di aggiornamento e il colore del mantello gel o lacca
Laminazione, incollaggio e tappatura perdite
Per il riempimento di piccole fessure e ubyt gemme in gelcoat
Una gamma di prodotti utili quando si lavora costruttore di barche