Wyszukaj na stronie

Parafina Sea-Line

Paraffin is an additive mainly to polyester gelcoats, necessary when it is necessary to apply the gelcoat to the outer surface of the finished laminate.

Gelcoat with the addition of paraffin corrector is topcot. By adding paraffin to the gelcoat, we will stop the phenomenon of oxygen inhibition, which is the reason why the gelcoat does not dry out and the surface remains sticky.

CapacityCode
60ml300010264
Parafina Sea-Line

Technical informations

Product description "Parafina Sea-Line"

  • Recommended amount of paraffin 2%-5%.
  • Mixing proportions of ingredients: gelcoat: hardener: paraffin 100:3:2-5

Always remember about health and safety.

  • Before working with chemical products, make sure you have read the SDS and TDS.
  • Use protective gloves, eye/face protection when handling the product, and wear a mask if instructed to do so.
  • Store the product in a tightly closed container at room temperature (15-25°C).
  • Protect from sunlight and frost.

You have questions about the product - Parafina Sea-Line

    Also check

    Our FAQ answers to frequently asked questions

    Can I use yacht paints for a drinking water tank?

    Sea-Line yacht paints are designed for painting the surface of boats and yachts made of various materials, e.g. laminate, wood or steel. We do not have a certificate of the National Institute of Hygiene, which would allow the use of yacht paint to paint the tank with drinking water.

    Why the paint does not have the right flow?

    Possible causes

    • No thinning, wrong thinner or wrong amount of thinner
    • Wrong type of roll or brush (wrong bristle lenght)
    • Applying too much or too Little paint,
    • During painting process temperature was too high or the air was too dry,
    • Incorrect preparation of too porous surface,
    • Incorrect proportion of thinner.

    How to prevent

    • Use a brush/Toller suited to the type of surface or paint,
    • Use thinner which is dedicated to the type of application and paints
    • Use thinning proportions which was indicated by manufacturer,
    • Paint in right atmosphere conditions indicated by manufacturer,

    How to remove

    • Grind, clean and paint again.

    Why the epoxy filler does not harden?

    Possible causes

    • Incorrect proportion of base and herdener,
    • Too low temperature of ambient and surface (less than 10ﹾC),
    • Mixing two components from two different manufacturers,

    How to prevent

    • Apply the correct proportions of components
    • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
    • Use base and hardener from the same manufacturer

    How to remove

    • The uncured mass requires complete removal from the surface.