Do you know that last year we modern epoxy fillers recipes?  To avoid confusions check on label if product is marked with ikon “new” or not. To find TDS and SDS cards please click this link DOWNLOAD.

Below differences for each Sea-Line epoxy filler.

.

.

.

.

Epoxy filler lightweight

 Epoxy filler lightweightOld recipeNew recipeDiffierences
ColorWhiteWhiteNo changes
Setting time24h20hA faster hardened product means faster readiness for further processing
Pot life 20C50 minutes50 minutesNo changes
Weight1L = 850 grams1L = 700 gramsLower product’s own weight
Proportions of mixingBy weight – 100:53

By volume – 2:1

By weight – 100:100

By volume – 1:1

Easier proportions of compounds mixing

Epoxy filler universal

Epoxy filler universalOld recipeNew recipeDiffierences
ColorGrayLight grayLighter shade of the new filler
Setting time5h15hLonger setting time
Pot life 20ﹾC10 minutes40 minutes30 minutes longer pot life
Weight1L = 1600 grams1L = 1540 gramsLower product’s own weight
Proportions of mixingBy weight – 100:44

By volume – 2:1

By weight – 100:50

By volume – 2:1

Easier proportions of compounds mixing

 

Epoxy filler with fibreglass

 Epoxy filler with fibreglassOld recipeNew recipeDiffierences
ColorLight greenLight grayColor changes
Setting time24h16hSetting time reduced
Pot life 20ﹾC25 minutes50 minutes25 minutes longer pot life
Weight1L = 1800 grams1L = 1550 gramsLower product’s own weight
Proportions of mixingBy weight – 100:50

By volume – 1:1

By weight – 100:50

By volume – 2:1

Easier proportions of compounds mixing

 

.

.

troton (37)

troton (40)


Partager:

Voir aussi
Autres threads de cette catégorie

Notre FAQ
Réponses aux questions fréquemment posées

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.

Can I use selfpolishing Sea-Line and HARD Sea-Line antifoulings on aluminium boat?

Sea-Line HARD and Sea-Line self-polishing antifouling are not intended for aluminum surfaces. They include copper oxide, which in contact with aluminum causes galvanic corrosion. Especially on aluminum, we offer ALU-PLUS self-polishing anti-fouling paint, which, in addition to excellent adhesion to aluminum, is also 30% more effective than traditional anti-fouling paints.

Can I add more hardener to speed up the reaction?

Do not add more hardener, because after the base has cured, the remaining hardener will react with subsequent layers, which will be applied to the surface and cause defects. For the product to work properly, please follow the proportions given by the manufacturer.