Wyszukaj na stronie

Our working hours during the virus threat

Since May 18th we change our working time. We are available from Monday to Friday from 8 a.m. to 3:00 p.m.

We are pleased to advise you what specific products will be useful for selected works, where to buy our products or how to become distributor for our products.

Our phone numbers (48) 604 821 461 and (+48) 94 35 316 75
We are also available by e-mail info@sea-line.eu

We continue to ensure the safety of employees and the continuity of our production plants. We take all preventive measures to reduce the risk of virus in our environment.

Our working hours during the virus threat

Also check

Our FAQ answers to frequently asked questions

Can I add some thinner to antifouling paint?

There is a possibility of thinning antifouling, but we do not recommend this procedure due to the risk of reducing the effectiveness of the paint. If it is necessary to thin the antifouling paint, it is recommended to dilute it to a maximum of 0-5% (by volume).

Why despite the use of antifouing paint the bottom of the boat is overgrown?

Possible causes

  • Too thin layer of antifouling paint,
  • Choosing the wrong antifouling to type of a boat or yacht
  • Thinning of antifouling paint,
  • Incorrect surface preparation before antifouling application.

How to prevent

  • Apply the right layer thickness of paint indicated by manufacturer,
  • Choose antifouling dedicated to type of boat or yacht and suitable for the type of water,
  • Do not thin antifouling because of the risk of reducing effectiveness,
  • Careful surface preparations (grinding, clearing, degreasing),

How to remove

  • Wet grinding, apply new layers of antifouling paint.
  • Use C1 shell and fouling remover.

Do you have to paint the scratched side of the boat?

If the scratches are not deep, then we can renew the scratched side by polishing with Sea-Line polishing pastes. Above the waterline, when the scratches are not deep, the surface can be repaired with a DRY FAST gel coat filler. Deep scratches should be filled with epoxy filler (selected depending on the requirements of the scratched surface), painted with a primer and then painted with topcoat.