Wyszukaj na stronie

METS Amsterdam 2021

Traditionally, from 16th to 18th November we would like to invite you to Amsterdam for the largest marine equipment and accessories trade fair (Marine Equipment Trade Show) – METS.

We are waiting for you at the Polish Pavilion in hall 5, stand 05.171

Why METSTRADE?

The METSTRADE Show is the world’s largest marine equipment trade show and the only truly international B2B exhibition for the industry.

The show has served as a platform for innovation, market developments and networking since the launch in 1988. It is a show every professional in the marine industry cannot miss.

  • Perfect place to network and forge profitable business relationships
  • Broad range of showcased innovations and new products
  • Unique B2B conference & seminar programme
  • Located in Amsterdam, one of the most beautiful cities in the world

See you at METS!

METS Amsterdam 2021

Also check

Our FAQ answers to frequently asked questions

Can I use selfpolishing Sea-Line and HARD Sea-Line antifoulings on aluminium boat?

Sea-Line HARD and Sea-Line self-polishing antifouling are not intended for aluminum surfaces. They include copper oxide, which in contact with aluminum causes galvanic corrosion. Especially on aluminum, we offer ALU-PLUS self-polishing anti-fouling paint, which, in addition to excellent adhesion to aluminum, is also 30% more effective than traditional anti-fouling paints.

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,