Wyszukaj na stronie

METS 2019 – largest marine equipment show

Traditionally, from 19th to 21th November we would like to invite you to Amsterdam for the largest marine equipment and accessories trade fair (Marine Equipment Trade Show) – METS.

We are waiting for you at the Polish Pavilion in hall 5, stand 05.271

Why METSTRADE?

The METSTRADE Show is the world’s largest marine equipment trade show and the only truly international B2B exhibition for the industry.

The show has served as a platform for innovation, market developments and networking since the launch in 1988. It is a show every professional in the marine industry cannot miss.

  • Perfect place to network and forge profitable business relationships
  • Broad range of showcased innovations and new products from 1,600 exhibitors
  • Unique B2B conference & seminar programme
  • Located in Amsterdam, one of the most beautiful cities in the world

See you at METS!

METS 2019 – largest marine equipment show

Also check

Our FAQ answers to frequently asked questions

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.

Why despite the use of antifouing paint the bottom of the boat is overgrown?

Possible causes

  • Too thin layer of antifouling paint,
  • Choosing the wrong antifouling to type of a boat or yacht
  • Thinning of antifouling paint,
  • Incorrect surface preparation before antifouling application.

How to prevent

  • Apply the right layer thickness of paint indicated by manufacturer,
  • Choose antifouling dedicated to type of boat or yacht and suitable for the type of water,
  • Do not thin antifouling because of the risk of reducing effectiveness,
  • Careful surface preparations (grinding, clearing, degreasing),

How to remove

  • Wet grinding, apply new layers of antifouling paint.
  • Use C1 shell and fouling remover.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.