Wyszukaj na stronie

TEAK OIL – NEW 2017

O1 Teak Oil is new product of brand Sea-Line which completes former offer products dedicated for wood protection.

O1 Teak Oil  is one-component oil for exotic wood. Oil for exotic wood which is difficult to impregnate; teak, mahogany, ipe wood, movingiu wood, etc. Excellent penetrating qualities into wood structure and does not leave any greasy layer on surface. O1 TEAK OIL protects wood from dampness and mold growth. It can be applied above and below the waterline as well as inwards it creates an isolating layer, easy in maintenance .

TEAK OIL – NEW 2017

O1 Teak Oil does not change the color of wood. Thanks that it can be used also in garden or home: garden furniture, terraces, parquet, windows,doors etc. O1 Teak Oil should be apply until overall saturation of wood is achieved.
O1 Teak Oil is available in volume 2,5 l and 250 ml. The smaller package was created for those clients which have small elements made of wood.

Theoretical output about 11-12 m2 per litre.

Also check

Our FAQ answers to frequently asked questions

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.
Wyjście