We are pleased to invite you to visit our YouTube channel. We’ve released new instant tutorial videos.

The main characters are gelcoat putty and polishing pastes.

Also check

Our FAQ answers to frequently asked questions

Why did the polyurethane topcoat become dull?

Possible causes

  • Too short time for evaporation of the thinner,

How to prevent

  • Maintain the right conditions for complete evaporation of the thinner,

How to remove

  • Mat the surface, degrease and apply the paint according to the rule (right conditions and thinning proportions)
  • Polish surface if needed.

Can I use selfpolishing Sea-Line and HARD Sea-Line antifoulings on aluminium boat?

Sea-Line HARD and Sea-Line self-polishing antifouling are not intended for aluminum surfaces. They include copper oxide, which in contact with aluminum causes galvanic corrosion. Especially on aluminum, we offer ALU-PLUS self-polishing anti-fouling paint, which, in addition to excellent adhesion to aluminum, is also 30% more effective than traditional anti-fouling paints.

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.