Wyszukaj na stronie

Labor Day May Holiday

Considering Polish National Holidays May 1th and May 3th our production and logistic will be closed those days.

In our industry, April and May is highest season, so for those who will need technical advice or info about nearest point of sale, please contact us:

April 27-30 from Monday till Thursday, call us from 6:30 a.m. to 1:00 p.m. and from 2:00 p.m. to 7:30 p.m.

May 4-8 from Monday till Friday, call us from 6:30 a.m. to 1:00 p.m. and from 2:00 p.m. to 7:30 p.m.

we are available at the following telephone numbers:
tel. (+48) 94 35 316 75;
tel. (+48) 94 35 316 79;
tel. (+48) 94 35 316 20;
info@sea-line.eu

For all of you around the world from all of us here at Sea-Line HAPPY LABOR DAY!

Labor Day May Holiday

Also check

Our FAQ answers to frequently asked questions

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,

Can I use universal thinner?

We do not recommend using universal thinners. The use of a thinner with an unknown composition may result in loss of adhesion, lack of proper flow of paint and varnish defects.