Wyszukaj na stronie

Boot Düsseldorf

Welcome to the 50th International Boat Show Düsseldorf, short boot is the world’s largest and most important international. Boat Fair takes place annually in January on the grounds of Messe Düsseldorf.

The boot Düsseldorf celebrates from 19.-27. January 2019 her 50th Anniversary: 50 years of magical moments and moving stories, 50 years of impressive boats and yachts, trends in all areas of water sports and 50 years of enthusiastic visitors who love the element of water.

We are particularly pleased to participate in the boat this year and celebrate 10 years of SEA-LINE in the anniversary year.
Celebrate with us and meet us at the booth of Yachticon A. Nagel GmbH in hall 11, booth 11 F10.

We look forward to seeing you!

More info >>> Boot Dusseldorf

Boot Düsseldorf

Also check

Our FAQ answers to frequently asked questions

Can I paint a boat, previously painted with 1 component paint, with polyurethane?

It is not recommended to apply 2K paints over 1K paints. 1K and 2K inks differ in their composition and properties, including hardness, chemical resistance and durability. 1K paints are one-component and dry by evaporating the solvent, while 2K paints are two-component and need to be cured by adding a hardener. Applying 2K paint over 1K paint can cause unpredictable chemical reactions and lead to undesirable effects such as dulling, chipping or flaking of the paint. Therefore, always use paints according to the manufacturer’s instructions and do not mix different types of paints. farby zgodnie z instrukcjami producenta i nie mieszać różnych rodzajów farb.

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.