Wyszukaj na stronie

Polishing cone is taking over control!

Polishing wool ball will be changed on cone shape.

Why shape of cone is more beneficial choice than ball? Because innovatory shape of cone :

  • allow us get to places which were practically unable to reach,
  • effectivity of polishing works are increasing.

Don’t be afraid! Polishing head in form of cone is as our other applicators:

  • is made in 100% from natural wool,
  • is dedicated to polishing gelcoats, tool gelcoats, paints and PU varnishes.

More info: info@sea-line.eu

Polishing cone is taking over control!

Also check

Our FAQ answers to frequently asked questions

Why did the polyurethane topcoat become dull?

Possible causes

  • Too short time for evaporation of the thinner,

How to prevent

  • Maintain the right conditions for complete evaporation of the thinner,

How to remove

  • Mat the surface, degrease and apply the paint according to the rule (right conditions and thinning proportions)
  • Polish surface if needed.

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.