Can I add more hardener to speed up the reaction?

Do not add more hardener, because after the base has cured, the remaining hardener will react with subsequent layers, which will be applied to the surface and cause defects. For the product to work properly, please follow the proportions given by the manufacturer.

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.

Why did the polyurethane topcoat become dull?

Possible causes

  • Too short time for evaporation of the thinner,

How to prevent

  • Maintain the right conditions for complete evaporation of the thinner,

How to remove

  • Mat the surface, degrease and apply the paint according to the rule (right conditions and thinning proportions)