Wyszukaj na stronie

Sea-Line News 2024

We are expanding our offer by introducing two new products that will provide boat enthusiasts and laminate processors with even greater possibilities in the field of repairs and construction. Here are our proposals.

Gelcoat in 250g and 1kg packaging:

Now available in two sizes – for both professionals and enthusiasts who need a flexible and durable material for repairs and construction. Our gelcoat features excellent adhesion, ensuring not only strength but also ease of use.

Sea-Line News 2024

Paraffin Corrector:

Here is our secret for even better results! The paraffin corrector that we can now offer adds a new quality to the process of working with laminates. The paraffin corrector will be particularly useful in the hands of enthusiasts engaged in small laminate repairs.

Application:

Both products are perfect for laminate processing as well as hobby use. They offer excellent quality and durability. In addition, they are an excellent choice for small repairs of laminate boats, providing not only the strength of repairs but also comfort in the area of processing.

Check out our new Sea-Line 2024 products!

Also check

Our FAQ answers to frequently asked questions

Can I paint the bottom of the boat with polyurethane paint?

Yes, you can paint the bottom of the boat with polyurethane paint due to its high mechanical strength. We recommend this solution when the boat is not launched for a long time and is not exposed to fouling.

Contamination in topcoat paint?

Possible causes

  • Inaccurate surface cleaning before paint application,
  • Incorrect painting tools preparation (brush and roll),
  • Performing work in a place exposed to constant contact with dust.

How to prevent

  • Careful surface preparation (grinding, clearing, degreasing),
  • Careful painting tools preparation before use,
  • Maintain clean work environment

How to remove

  • Grind, clean and paint again.

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.