SILVER CRUISE POLISHING ANTIFOULING

Accueil » Produits » Peinture antifouling » SILVER CRUISE POLISHING ANTIFOULING
Szpachlówki i podkłady szkutnicze
SILVER CRUISE POLISHING ANTIFOULING


Use biocides safely. Always read the label and product information before use.

TypeGRP laminates, wood, steel
PlaceBelow waterline
Function Antifouling paint discourages the growth
of barnacles, weed, and other water life on the submersed hull of the boat.
Application brush, roll

airless spray gun (only professional)

Thinning *No recommended
Theoretical coverage For 1lby rollerby spray
9 ~ 10 m²3 ~ 5 m²
Coat thickness (WTF)98 μm196 μm
Finish thickness (DTF)50 μm100 μm
Coats number21
Recommended dry layer100 μm
Hardening the surfaces23ºC15ºC
Touch dry30 minutes45 minutes
Immersion:4 hours6 hours
Dry to recoat (overcoating)min. 6 hoursmin. 10 hours
Dry to launch (immersion times)max 6 monthsmax 6 months
Pack0,75 l2,5 l
Color **codecode
white

red

blue

navy

black

300008388

300008390

300008392

300008394

300008396

300008387

300008389

300008391

300008393

300008395

* THINNING NOTICE:

In the case of high temperatures and the need to thin the antifouling paint, a maximum dilution of 0-5% (by volume) is recommended.
Dilution and the application method directly affect the thickness of the antifouling paint layer.

Special attention should be paid to obtaining a specific coating thickness (100 μm DTF), which ensures the effective operation of the antifouling paint.

** COLOR NOTICE:

Exposure of a freshly applied antifouling paint to moist air can lead to color change. The discoloration is only superficial and does not affect the effectiveness of the antifouling paint. Due to the content of copper oxide, a small color difference between the parts of the antifouling paint is acceptable.

Antifouling available only in:


Partager:

Avez-vous des questions?
Nous vous répondrons dans les plus brefs délais
 
Voir aussi
Autres produits de cette catégorie

Notre FAQ
Réponses aux questions fréquemment posées

Contamination in topcoat paint?

Possible causes

  • Inaccurate surface cleaning before paint application,
  • Incorrect painting tools preparation (brush and roll),
  • Performing work in a place exposed to constant contact with dust.

How to prevent

  • Careful surface preparation (grinding, clearing, degreasing),
  • Careful painting tools preparation before use,
  • Maintain clean work environment

How to remove

  • Grind, clean and paint again.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.