GELCOAT FILLER “DRY FAST”

PRODUCT DISCRIPTION :

NEW Gelcoat Filler is very fast hard and easy in use.


BASIC INFORMATION :

TypeGRP Laminates
PlaceAbove waterline
FunctionScratches and small repairs
Pot life 20°C6÷7 min
Hardening time 20°C4 h

PACKAGING:

CODE:

250g

100g

APPLICATION METHODS:

Manually:

Technical information:

GELCOAT FILLER „DRY FAST” (styrene free):


Share:

Do you have any questions?
We will respond as soon as possible

Related products

from GELCOAT FILLER “DRY FAST”


See also
Other products in this category

Our FAQ
Answers to frequently asked questions

Why did the polyurethane topcoat become dull?

Possible causes

  • Too short time for evaporation of the thinner,

How to prevent

  • Maintain the right conditions for complete evaporation of the thinner,

How to remove

  • Mat the surface, degrease and apply the paint according to the rule (right conditions and thinning proportions)
  • Polish surface if needed.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.