Language:

Polyurethane Topcoat – color

Home » Products » Topcoats » Polyurethane Topcoat – color
Naprawa łodzi
Polyurethane Topcoat – color


TypeLaminates GRP, wood, steel, aluminum
PlaceAbove waterline
FunctionHigh gloss top coat
Applicationbrush, roll, spray gun
ThinningRoll/ brush thinner for PU

or

Spray thinner for PU

Theoretical coverage For 1l13-14 m2 for 75 μmWFT/ 40 μm DFT
Number of coats1 – 3
Pot life 20°C3 h
Time between layers without sandingminimum 30 minutes
Pack0,750l15 l
Color:code:
White56536222
Light ivory56577727
Ruby red5656X
Sapphire blue56557779
Sky blue81638162
Mint green7322X
Squirrel grey74387439
Jet black62627994

ROLLER / BRUSH

SPRAY

During paint job is recommend to use products from one batch

Farba-poliuretanowa


Share:

Do you have any questions?
We will respond as soon as possible

Related products

from Polyurethane Topcoat – color


See also
Other products in this category

Our FAQ
Answers to frequently asked questions

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.

Why did the polyurethane topcoat become dull?

Possible causes

  • Too short time for evaporation of the thinner,

How to prevent

  • Maintain the right conditions for complete evaporation of the thinner,

How to remove

  • Mat the surface, degrease and apply the paint according to the rule (right conditions and thinning proportions)
  • Polish surface if needed.

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.