Language:

Fouling Stop SEAGUARD

Home » Products » Antifouling paints » Fouling Stop SEAGUARD
Naprawa łodzi
Fouling Stop SEAGUARD

Fouling Stop SEAGUARD – a new anti-fouling paint for hulls.


TypeGRP laminates, wood, Steel, aluminium
PlaceBelow waterline
FunctionAntifouling paint discourages the growth
of barnacles, weed, and other water life on the
submersed hull of the boat.
Applicationbrush, roll, spray gun
Thinning *No
Theoretical coverage For 1l9÷10 m2 for 100 μmWFT/ 50 μm DFT
Coats number1 – 3
Time between layersMin 5 h
Dry to launch:Min 12 h – max 30 day
Pack0,750 l  2,5 l
Color **:

white

dark blue

black

code:

300009843

300009836

300011250

code:

300009847

300009846

300011251

* THINNING NOTICE:

In the case of high temperatures and the need to thin the antifouling paint, a maximum dilution of 0-5% (by volume) is recommended.
Dilution and the application method directly affect the thickness of the antifouling paint layer.

Special attention should be paid to obtaining a specific coating thickness (100 μm DTF), which ensures the effective operation of the antifouling paint.

** COLOR NOTICE:

Exposure of a freshly applied antifouling paint to moist air can lead to color change. The discoloration is only superficial and does not affect the effectiveness of the antifouling paint.

Technical information:


Share:

Do you have any questions?
We will respond as soon as possible
 
See also
Other products in this category

Our FAQ
Answers to frequently asked questions

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.

Do you have to paint the scratched side of the boat?

If the scratches are not deep, then we can renew the scratched side by polishing with Sea-Line polishing pastes. Above the waterline, when the scratches are not deep, the surface can be repaired with a DRY FAST gel coat filler. Deep scratches should be filled with epoxy filler (selected depending on the requirements of the scratched surface), painted with a primer and then painted with topcoat.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,
Our offer
Familiarize yourself with our offer of boatbuilding materials and paints
Exit