Polishing systems meet all stages of production, as well as during repair work, renovations or treatments. Different hardness of materials, colors and expected finish level require the use of different cutting force polishing compounds and specialized heads, sponges or fur.

The table shows the proper selection of Sea-Line polishing compounds for various types of polishing heads.

PRODUCT :SEA-LINE®
S0
SEA-LINE®
SO5
SEA-LINE®
S1
SEA-LINE®
S1 PREMIUM
SEA-LINE®
S2
CUTTING FORCE8 / 109 / 106 / 108 / 102 / 10
GLOSS LEVEL6 / 108 / 106 / 89 / 1010 / 10
PAPER GRADATIONBRIGHT COLOURS AND SURFACES OF LOW OR AVERAGE HARDNESS
P800⇒P800⇒P1200⇒P800⇒P3000⇒
DARK COLOURS AND SURFACES OF HIGH HARDNESS
P1200⇒P1200⇒P1500⇒P1200⇒P3000⇒
MATERIALS DIFFICULT TO POLISH (PLEXI, POLICARBONATES)
XP1500⇒P2000⇒P1500⇒X
UV PROTECTION LEVELXXVERY LOWXAVERAGE
MANUAL LABOUR
ROTARY MACHINE
ORBITAL MACHINEOPTIONAL

( P2000⇒)

OPTIONAL

( P2000⇒)

XOPTIONAL

( P2000⇒)

TYPE OF SURFACES
TOOL GELCOATX
GELCOAT
POLYURETHANE PAINTSXOPTIONAL
INDUSTRIAL PAINTS
OTHER PAINTSOPTIONAL
PLEXI, POLICARBONATESOPTIONALOPTIONAL
CHOOSING APPROPRIATE APPLICATOR SEA-LINE®
SHEEP WOOL FOR GELCOAT SEA-LINE®
X
SHEEP WOOL POLISHING BALL (∅80mm)X
LAMBSWOOL TYPE D
X
LAMBSWOOL TYPE mm
“BRAYT „PROFI” POLISHING SPONGE
X
“BRAYT „FINISH” POLISHING SPONGE
POLISHING SPONGEWHITE
X
PINK
X
YELLOW
BLACKXX

Share:

Do you have any questions?
We will respond as soon as possible
 
See also
Other products in this category

Our FAQ
Answers to frequently asked questions

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.
Our offer
Familiarize yourself with our offer of boatbuilding materials and paints
Exit
Przewiń na górę