New in offer product S0 – Brayt Sea-Line is polishing paste designed for professionals – companies producing molds and products where the outer layer of the gel coat or industrial topcoat with a high degree of hardness.
S0 removes defects after sanding grit sandpaper even P800 (depending on the hardness of the surface).
Pasta machine is designed to work. Machining maximum speed of 1800 RPM.
Brayt S0 cooperating with wool applicators, and made ​​of hard sponges. We get a surface gloss.
Pastes BRAYT Sea-Line does not contain silicones or fillers which mask features temporarily. Due to such pastes BRAYT Sea-Line is stable and does not go away after wiping the surface with acetone;)
Package 1kg .

Μετοχή:

Δείτε επίσης
Άλλα νήματα σε αυτήν την κατηγορία

Οι συχνές ερωτήσεις μας
Απαντήσεις σε συνήθεις ερωτήσεις

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,

Contamination in topcoat paint?

Possible causes

  • Inaccurate surface cleaning before paint application,
  • Incorrect painting tools preparation (brush and roll),
  • Performing work in a place exposed to constant contact with dust.

How to prevent

  • Careful surface preparation (grinding, clearing, degreasing),
  • Careful painting tools preparation before use,
  • Maintain clean work environment

How to remove

  • Grind, clean and paint again.

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.