YACHT VARNISH 1K

Home » Prodotti » Smalti e Vernici » YACHT VARNISH 1K
Szpachlówki do łodzi
YACHT VARNISH 1K


Typewood
PlaceAbove waterline, interior
FunctionHigh gloss
Applicationbrush, roll, spray gun
ThinningThinner for 1 – component primer, varnisch, enamel
Theoretical coverage for 1l12-13 m2 for 80 μm WFT/ 40 μm DFT
Number of coats1 ÷ 3 – renewal old varnish

1 ÷ 5 – new wood, creating new coat

Dry to the touch 20°C:3 h
Dry to rain 20°C:16 h
Fully woterprof24 h
Elapsed time before applying next coat:min. 16 h
Color:transparent
Pack :0,750 l
Code:300008170

Condividi:

Avete domande?
Ti risponderemo il prima possibile

Prodotti correlati

da YACHT VARNISH 1K


Vedi anche
Altri prodotti in questa categoria

Le nostre FAQ
Risposte alle domande più frequenti

Why despite the use of antifouing paint the bottom of the boat is overgrown?

Possible causes

  • Too thin layer of antifouling paint,
  • Choosing the wrong antifouling to type of a boat or yacht
  • Thinning of antifouling paint,
  • Incorrect surface preparation before antifouling application.

How to prevent

  • Apply the right layer thickness of paint indicated by manufacturer,
  • Choose antifouling dedicated to type of boat or yacht and suitable for the type of water,
  • Do not thin antifouling because of the risk of reducing effectiveness,
  • Careful surface preparations (grinding, clearing, degreasing),

How to remove

  • Wet grinding, apply new layers of antifouling paint.
  • Use C1 shell and fouling remover.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.