„…  It was not easy,  hard job on knees with mask and glasses. Feeling like 40 years ago during military trainings.

Sea-line products (as most of modern paints) let’s amatours for quiet good application. Now my yacht Sombra Blanca has best bottom on the world. In few weeks I’m going to be back on the water”

Witold /Wrocław

<<< FULL RELATION >>>


Partager:

Voir aussi
Autres threads de cette catégorie

Notre FAQ
Réponses aux questions fréquemment posées

Can I add more hardener to speed up the reaction?

Do not add more hardener, because after the base has cured, the remaining hardener will react with subsequent layers, which will be applied to the surface and cause defects. For the product to work properly, please follow the proportions given by the manufacturer.

Can I degrease surfaces with acetone?

We do not recommend degreasing the surface with acetone, because acetone evaporates very quickly, which affects the quality of cleaning the painted surface.

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.