GELCOAT FILLER « DRY FAST »

Accueil » Produits » Mastics » GELCOAT FILLER « DRY FAST »
Farby szkutnicze
GELCOAT FILLER « DRY FAST »

PRODUCT DISCRIPTION :

NEW Gelcoat Filler is very fast hard and easy in use.


BASIC INFORMATION :

TypeGRP Laminates
PlaceAbove waterline
FunctionScratches and small repairs
Pot life 20°C6÷7 min
Hardening time 20°C4 h

PACKAGING:

CODE:

250g

100g

APPLICATION METHODS:

Manually:

Technical information:

GELCOAT FILLER „DRY FAST” (styrene free):


Partager:

Avez-vous des questions?
Nous vous répondrons dans les plus brefs délais

Produits connexes

de GELCOAT FILLER « DRY FAST »


Voir aussi
Autres produits de cette catégorie

Notre FAQ
Réponses aux questions fréquemment posées

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.