Tipo de embarcaciónlaminado, madera, acero, aluminio
LugarPor encima por debajo de la linea de flotación
FunciónReparaciones por encima de la linea de flotación y en exterior
AplicaciónA mano/ éspatula
Tiempo de trabajo 20°C3-5 min
Tiempo de secado 20°C20 ± 30 min
Color :
UNIVERSAL

LIGERA

CON FIBRA DE VIDRIO

Blanco

Crema

Marrón

EMBALAJE :

MASILLAS DE POLIÉSTER

UNIVERSAL :

MASILLAS DE POLIÉSTER

LIGERA :

MASILLAS DE POLIÉSTER

FIBREGLASS :

Información técnica:

MASILLAS DE POLIÉSTER

MASILLAS DE POLIÉSTER (low styrene)

Polyester filler universal

Polyester filler lightweight

Polyester filler with fiberglass

Polyester filler universal

Polyester filler with fiberglass


Compartir:

¿Tienes alguna pregunta?
Le responderemos lo antes posible

Productos relacionados

de MASILLAS DE POLIÉSTER: UNIVERSAL, LIGERA, CON FIBRA DE VIDRIO


Ver también
Otros productos de esta categoría

Nuestras FAQ
Respuestas a las preguntas más frecuentes

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.

Can I use selfpolishing Sea-Line and HARD Sea-Line antifoulings on aluminium boat?

Sea-Line HARD and Sea-Line self-polishing antifouling are not intended for aluminum surfaces. They include copper oxide, which in contact with aluminum causes galvanic corrosion. Especially on aluminum, we offer ALU-PLUS self-polishing anti-fouling paint, which, in addition to excellent adhesion to aluminum, is also 30% more effective than traditional anti-fouling paints.

Contamination in topcoat paint?

Possible causes

  • Inaccurate surface cleaning before paint application,
  • Incorrect painting tools preparation (brush and roll),
  • Performing work in a place exposed to constant contact with dust.

How to prevent

  • Careful surface preparation (grinding, clearing, degreasing),
  • Careful painting tools preparation before use,
  • Maintain clean work environment

How to remove

  • Grind, clean and paint again.
Nuestra oferta
Consulte nuestra oferta de materiales y pinturas para la construcción de embarcaciones
Exit
Przewiń na górę